Post by captfue on Sept 24, 2015 12:03:23 GMT -5
|
|
|
Post by Leon on Sept 24, 2015 12:45:00 GMT -5
WOW!!!!That is awesome looking work.
|
|
|
Post by deafpanzer on Sept 25, 2015 8:46:31 GMT -5
Melted sprue!?!? WOW! Great start... got my seat and popcorn!
|
|
|
Post by wbill76 on Sept 25, 2015 19:28:31 GMT -5
The ultimate recycling program! He looks good so far.
|
|
John Everett
Full Member
Member since: January 2012
July, 2016 MoM Winner
Posts: 1,278
Jan 17, 2012 0:53:48 GMT -5
Jan 17, 2012 0:53:48 GMT -5
|
Post by John Everett on Sept 25, 2015 19:34:06 GMT -5
Wow! What are you using to melt the sprue? I read somewhere that the solvents were no long sold to the public, something about growing a third eyeball.
|
|
captfue
Full Member
Member since: October 2012
Posts: 311
Oct 1, 2012 22:25:19 GMT -5
Oct 1, 2012 22:25:19 GMT -5
|
Post by captfue on Sept 27, 2015 16:14:10 GMT -5
No I don't use any solvents. I use heat from a soldering iron to melt the sprue..I've got some more WIP shots I post in a bit
|
|
captfue
Full Member
Member since: October 2012
Posts: 311
Oct 1, 2012 22:25:19 GMT -5
Oct 1, 2012 22:25:19 GMT -5
|
Post by captfue on Oct 22, 2015 16:23:37 GMT -5
Here are some up dated pictures
|
|
|
Post by deafpanzer on Oct 23, 2015 14:59:43 GMT -5
No pictures here. I am anxious to see the update.
|
|